Galvanic Corrosion
Electrochemical corrosion that occurs when dissimilar metals are electrically connected in an electrolyte such as seawater.
The less noble metal becomes anodic and corrodes preferentially. Material selection, electrical isolation, coatings and correctly designed sacrificial anodes help control the process without replacing inspection and maintenance.